ZHU Dantong, WU Qian, LI Wenfei, et al. Preparation and properties of kaolin grafted alkyl amine type dripping agent/polyethylene composites[J]. Acta Materiae Compositae Sinica, 2020, 37(1): 35-41. DOI: 10.13801/j.cnki.fhclxb.20190416.002
Citation: ZHU Dantong, WU Qian, LI Wenfei, et al. Preparation and properties of kaolin grafted alkyl amine type dripping agent/polyethylene composites[J]. Acta Materiae Compositae Sinica, 2020, 37(1): 35-41. DOI: 10.13801/j.cnki.fhclxb.20190416.002

Preparation and properties of kaolin grafted alkyl amine type dripping agent/polyethylene composites

  • The eighteen alkyl diethanolamine acrylic monoester dripping agent (AAM) was grafted onto kaolin (Ka) by surface grafting, the grafting of AAM and Ka (Ka-g-AAM) was prepared. Then Ka-g-AAM/linear low density polyethylene (LLDPE) composites were prepared by melt extrusion. The structure and properties of Ka-g-AAM/LLDPE were investigated by FTIR, SEM, DSC and acceleration dripping testing etc. The results indicate that AAM is grafted onto the surface of Ka. Compared with AAM/LLDPE and Ka-AAM/LLDPE composite, Ka-g-AAM/LLDPE composites have inconspicuous changes on the melting temperature, the crystallization temperature and mechanical properties. The acceleration dripping duration of Ka-g-AAM/LLDPE composite films is 23 days at 60℃, which is 4 days longer than that of AAM/LLDPE composite.
  • loading

Catalog

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return